Wanted some ideas on where you guys would send an HK416 upper to get refinished? I was thinking robar finish, but was told they would not be able to keep any markings (white) they all would be coated over so all markings would be black once its completed.

Any ideas/suggestions?

thanks
 

·
Registered
Joined
·
593 Posts
try US Anodizing (contact name is Victor)

they do awesome work and about a 2 week turn around time

not sure about saving the lettering etc though
 

·
Registered
Joined
·
527 Posts
Get it finished any way you like, then buy a laquer stik from Brownells and fill in the lettering yourself. Done!
 